Previous Icon 3

Next Icon 3

Micropitting (frosting)

Calculation method

The calculation is performed according to ISO 15144, Method A. All the required data is taken from the contact analysis.

Lubrication gap thickness h and specific thickness of lubrication film λGFP

The calculation of the progression of the effective lubrication gap thickness h and the effective specific lubrication gap thickness λGF across the meshing is precisely defined in the ISO TR 15144 proposal. The lubrication gap can vary significantly depending on local sliding velocity, load and thermal conditions. The location with the smallest specific lubrication gap thickness is the decisive factor in evaluating the risk of micropitting.

Permitted specific thickness of lubrication film λGFP

To evaluate the risk of micropitting (frosting), it is vital that you know how large the required smallest specific lubrication film λGFmin is to be. The calculation rule states that:

λGFmin >= λGFP to prevent micropitting (frosting), or to ensure safety against frosting Sl = λGFminP/ λGFP.

If the lubricant's micropitting load stage is known, the permitted specific lubricant film thickness is calculated according to ISO TR 15144.

Otherwise, reference values for λGFP can be obtained from the appropriate technical literature.

In [81] you will see a diagram that shows the permitted specific lubrication gap thickness λGFP for mineral oils, depending on oil viscosity and the micropitting (frosting) damage level SKS.

18-grafik_micropitting

Figure 22.13: Minimum necessary specific thickness of lubrication film λGFP

The micropitting damage level SKS, determined according to FVA information sheet [82], is nowadays also stated in data sheets produced by various lubricant manufacturers. The data in the diagram applies to mineral oils. However, synthetic oils with the same viscosity and micropitting (frosting) damage level show a lower permitted specific lubrication film λGFP [81]. Unfortunately, as no systematic research has been carried out on its effects, no properly qualified values are available.

Furthermore, you must be aware that the predefined values λGFP only apply to case-hardened materials. As specified in ISO TR 15144, for other materials, the permitted specific lubrication gap thickness λGFP can be multiplied by the coefficient Ww.

 

Ww

Case hardening steel, with austenite content <= 25%

1.00

Case hardening steel, with austenite content > 25%

0.95

Gas-nitrided (HV > 850)

1.50

Induction or flame-hardened

0.65

Through hardening steel

0.50

Table 22.1: Material coefficient

It is interesting to note that, at least according to the table shown above, materials with a nitrite content are more prone to micropitting (frosting) than case hardened materials when the same lubrication gap is used. In contrast, through hardened materials that are not surface hardened are much more resistant.

You should be aware that the data shown here must be used with caution, because information about the micropitting (frosting) process is still incomplete, and even technical publications will sometimes contain contradictory data.

Safety against micropitting

If the load stage against micropitting as defined in FVA C-GF/8.3/90[82] is specified for the lubricant, the minimum required lubricant film thickness λGFP is calculated. The safety against micropitting can therefore be defined as Sλ = λGFmin/ λGFP.